Never done a knuckle rebuild but I’d have to guess the inside of the axle housing shouldn’t look boogered up and scarred.
The axle is supposedly a ‘78. This is the driver’s side and i had absolute hell getting the knuckle bearings off the bearing caps.
All that to say…
Shouldn’t the inside of this housing look machined and not like a bad weld job? Cracks, scarring, etc. Opinions?
The axle is supposedly a ‘78. This is the driver’s side and i had absolute hell getting the knuckle bearings off the bearing caps.
All that to say…
Shouldn’t the inside of this housing look machined and not like a bad weld job? Cracks, scarring, etc. Opinions?