I was in North Van for almost 3 months at seaspan working on the new joint support ship for the navy.. came back to Vic mid December.. been working like crazy here.. just did 21 days straight 10s .. what's you been up too...
Side note for bending aluminium. . 5052 is used for bending .. 6061 structural. . Difference is how they are treated when made.. 6061 age hardens..
As for bending .. bend against the grain of the aluminium. . If your bend is with the grain of the aluminum it will Crack. .. this is also...
Been awhile since I did anything with my 40.. so thought it was time to due some upgrades.. bought a headlight kit from toyota after reading a couple threads and getting a part number for it..
Funny thing was asking the parts guy at toyota about the upgrade kit.. soon as I said 73 fj40 he...