RUSH55
SILVER Star
Sprayed some single stage acrylic urethane at its recommended viscosity (no more than 10% reduction) on the roof of my 55 which resulted in gnarly orange peel. After waiting for the appropriate time I started color sanding in an effort to knock everything down flat. What I began finding was this micro porosity in the paint. Haven’t talked to the “rep” yet as I’m trying to get things corrected on my own first. Can anyone tell me what the possible causes could be for this condition and what some possible fixes could be, shy of a complete re-strip and re coat?
First pic shows the orange peel
Second pic shows how much it needed to be knocked down
Third pic shows the porosity (might need to zoom in to see it)
First pic shows the orange peel
Second pic shows how much it needed to be knocked down
Third pic shows the porosity (might need to zoom in to see it)