Getting paint to stick to galvanized metal is quite a challenge. Ford had trouble with this in the 1970s - look at the cowl on pickups of that era. There are a number of post-galv. steps to getting paint to stick. YMMV.
This is a 1975 Ford that sat in a field since the 80s.

8C698847-0BF0-48D8-8CD7-58E231FFAEBE.webp
 
You treat new galvanized metal with T-wash, Then you paint it with a self etching primer than you can use a high build primer and the paint of your choice. The appeal for me is that after sandblasting all of the paint off they put it in an acid bath and prep the metal so all of the hidden rust gets cleaned and washed and then the galavinization gets into every, nook, cranny, channel, tube etc. where rust can hide and start all over again.
Sending my frame for galvanizing next week. Where did you buy the T-wash?
 
Yes done it. Before you do so install bolts in all the threaded holes. When you get it back pull the bolts and you may have to rethread possibly. Use anti-seize on all bolts going into the frame or just in general.
 
Yes done it. Before you do so install bolts in all the threaded holes. When you get it back pull the bolts and you may have to rethread possibly. Use anti-seize on all bolts going into the frame or just in general.
Careful, if they are over the thread inside, you can’t get them out!
 
T-wash is a British product. If you can't get it you can use phosphoric acid. Apply the phosphoric acid let it set for 20 to 30 minutes than wash it off,
 