I have my axles apart for a complete replacement of all the bearings. I want to get it hot tanked/acid bath (same thing?) to get in clean so I can powdercoat the axle housing.
I'm not having any luck finding machine shops locally that can do it. What should I search under? Would it be machine shops, electroplating shops, some sort of heavy vehicle shops????

I'm in Jacksonville Fl, so if anyone knows someone around here, that would be awesome.

Thanks.
 
Radiator shops will do things besides radiators (ie gas tanks) Maybe you can talk somebody into it.

Your powder coater should have snad/media blasting capabillites
 
Kofoed said:
Radiator shops will do things besides radiators (ie gas tanks) Maybe you can talk somebody into it.

Your powder coater should have snad/media blasting capabillites


Ja, most PC places will want to put it through their own prep before they coat it.
I'd call the place and see what they need. You might get the grease off of it but that may be all they want.

GL

Ed
 
There's a guy next door who has a powdercoating business and ALSO drives an FJ-40 :eek: :D. He also does sandblasting.

He's going to blast my frame. he told me that with the grease and whatnot on the axle housing, the blaster sometimes forces it into the metal and then it bubles out and messes up the powdercoat.

I'm going to try to 1.) Hot tank it or 2.) have it steam cleaned with a good degreaser.

One thing I found while searching has me REALLY excited and I'm gettting a quote on my body tub and frame :eek: :eek: :eek: (it looks like they can "hot tank" and then some......)

EDIT: had a link to a company that does large-size galvanizing (a cruiser tub would fit) but they won't do vehicles :mad: I have some calls out to a few other places. I was psyched about hot-dip galvanizing my whole body, but it isn't looking so good now.... :mad:
 
Last edited:
There's a place in Portland, OR that will hot dip anything up to and including a car chassis. They have really big tanks. The process leaves protetive coating on the outside of the metal. Check out metal restoration shops in your area.
 
Had a relative that did that to a car body, the acid removes everything from everywhere, then they rinse and do a phosphate dip, if you have factory seam sealer between spotwelded seams, that goes too. it turned out nice, but he expects the car to rattle more and leak.
 
Hemmings Motor News had some sources for the whole body:

Chem-strip in Carolina (www.chem-strip.com) and Restoration Depot in S. Florida (http://www.restorationdepot.net/ web site links don't work, but the contact information is on there)are the two nearest me. Restoration Depot quoted me $1000 to strip just the tub. sounded like a lot, but they do say it will remove EVERYTHING that isn't steel (including all rust). I figure the time/hassle of doing it yourself may make it worth the $ to get a really thorough job done.

I did find a machine shop in town that will hot-tank parts, including motors, axle housings etc. The hot-tanking only removes grease, it won't remove paint or rust ( so those parts will need to be sand-blasted afterwards)

GALVANIZING: I found a place in Georgia that can hot-dip galvanize frames and bodies. They say there is a risk of distortion when dipping bodies. I'm going to get my frame dipped before I paint it. I'm also pretty certain to be getting a Panama steel tub and I'm going to have them galvanize that before I paint it :D :D :D Once I get this underway I'll post on how much it is to do a frame/body.

There aren't many galvanizers willing to work with automotive stuff. I called a few (including one that is only 40 min from my house :mad: )but they said they wouldn't do my 'Cruiser parts.
The place that will is: http://www.southatlanticllc.com/ga.htm, they seemed very helpful.

Summary: I may take my cowl/fenders/bib/hood to South Florida to get stripped. I'm definately getting my frame and almost for sure my tub hot-dipped galvanized. I will keep everyone posted on the costs/results of this.
 
His was a car body, and he had several panels that were seam sealed between spot welded flanges, now they are loose as the filler took up some room, kind of hard to get seam sealer between welded panels. As far as galvanizing, I would say that distortion is more than a worry, it's a definite. thin panels will warp, thicker parts will warp. we have stuff hot dip galvanized all the time, and it's really hot. we've gotten back tanks that are warped out of shape, even tubes that are thick enough and strong enough get bent when they occasionally set them down a little hard out the tank, plus they don't want to do anything that won't drain completely out.

i wonder if you could do a cold process, copperplate or maybe even chrome it. might be safer on the body.

the most practical would be the phosphate dip most acid dippers use, it's much better than bare steel for corrosion, and it provides a good adhesion coat for powdercoat and paint, and it won't warp panels.
you can buy it in a brush on type if you sandblast your own body, but we haven't done much testing with this method.
I would skip the galvanize and go with the phosphate.
 
I think that caustic (the opposite of acidic) removes grease and paint, etc, and acid removes everything, including rust and some of the base metal, which may not be good for a machined part.

I would recomend doing a web search for draino (the pipe stuff).
 
FoYoChe said:
els. As far as galvanizing, I would say that distortion is more than a worry, it's a definite. thin panels will warp, thicker parts will warp.

I was thinking about taking a fender or hood to have it dipped to see if it does get distorted. Kinda to test the process before taking a chance on my tub. I'll need to look into it a lot before committing to the tub. I'm definately going to get the frame done...

How do they galvanize things like raw sheetmetal, metal garbage cans etc. without distorting? Do they use a cold process for that stuff?
 