PIG is going to work. If I mig weld it I will use 98-2. I might tig this one. May take longer but will look much nicer. Jmack knows.Use a 308/308L filler material and use a tri-mix shielding gas or an argon blend such as 98-2 Ar-O2 or 95-2/95-5 Ar-CO2 and it should work just fine.
Jmack knows. PIG is going to work. So if I mig it will be 98-2. I think I am going to Tig will look much nicer.Use a 308/308L filler material and use a tri-mix shielding gas or an argon blend such as 98-2 Ar-O2 or 95-2/95-5 Ar-CO2 and it should work just fine.
TriedThis is amazing. But you got me thinking... If you are going through all the trouble of making a bunch of patch panels, cutting, welding, grinding etc. Might be less work in the long run to fly to Japan and find the fj55 body press blanks and just make the entire pig out of stainless. Might be heavier but they don't call it a pig for nothing! I bet it would take less time...